MatWeb, The Online Materials Database
PolyOne Geon® 8700A Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Interior
- Excellent Dimensional Stability
- High Melt Strength
- UL 94 V0
- UL 94 5VA
- CSA V0
- NSF STD 51
Applications: - General Purpose
- Custom Profiles-Complex
- Custom Profiles-Thick wall
- Beltline Moldings
Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.38 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Rockwell R | 111 | ASTM D785 |
Hardness, Shore D | 78 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 6200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 390000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 380 ksi | ASTM D790 |
Flexural Strength | 11000 psi | ASTM D790 |
Compressive Strength | 8100 psi | ASTM D695 |
Dart Drop Total Energy | 0.07 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 0.07 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 1.1 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 0°F (-18°C); ASTM D256 |
Izod Impact, Notched | 1.6 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 32°F (0°C); ASTM D256 |
Izod Impact, Notched | 17 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Electrical Properties |
|
Dielectric Constant | 3.3 | 1,000 Hz; ASTM D150 |
Dielectric Constant | 3.9 | 60 Hz; ASTM D150 |
Dielectric Strength | 690 V/mil | ASTM D149 |
Dissipation Factor | 0.029 | 60 Hz, 86°F (30°C), 24 hrs; ASTM D150 |
Dissipation Factor | 0.04 | 1,000 Hz, 86°F (30°C), 24 hrs; ASTM D150 |
Thermal Properties |
|
CTE, linear 68°F | 37 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 163 °F | Unannealed, 0.125 in bars; ASTM D648 |
Flammability, UL94 | V-0 | All Colors; 0.028 in. |
Flammability, UL94 | V-0 | All Colors; 0.034 in. |
Flammability, UL94 | 7 | All Colors; 0.059 in. |
Processing Properties |
|
Melt Temperature | 355 - 360 °F | Extrusion |
Descriptive Properties | |
Automotive Approval | General Motors, GMP 7001M PVC | |
Cell Classification D1784 | 16344 | ASTM D1784 |
Ease of Sizing | Excellent | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|