PolyOne Geon® 8700X Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Very Good Dimensional Stability
  • High Melt Strength
  • UL 94 5VA
  • UL 94 V0
  • CSA V0
  • CSA 5VA
  • NSF STD 51

Applications:

  • Custom Profiles-Thick wall
  • Beltline Moldings

Market:

  • Automotive

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: Automotive OEM approval(s).
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.
Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.38 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D79 15 sec; ASTM D2240
Tensile Strength, Yield6100 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus360000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus360 ksi ASTM D790
Flexural Strength11000 psi ASTM D790
Dart Drop Total Energy0.1 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.1 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched18.9 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched20.3 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched20.6 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F37 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)164 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0 All Colors; 0.03 in.
Flammability, UL94V-0 All Colors; 0.036 in.
Flammability, UL947 All Colors; 0.062 in.
Flammability, UL947 All Colors; 0.075 in.

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
Automotive ApprovalGeneral Motors, GMP 7001M PVC 
Cell Classification D178416344 ASTM D1784
Ease of SizingExcellent 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.