MatWeb, The Online Materials Database

PolyOne Geon® 87018 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Cellular

Applications:

  • Horizontal Blinds

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.
NOTE: Physical Properties were measured on flat cellular profiles with a 0.72 specific gravity natural compound.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity0.6 - 0.75 g/cc0.0217 - 0.0271 lb/in³ Cellular; ASTM D792

Mechanical Properties
Hardness, Shore D7373 15 sec; ASTM D2240
Tensile Strength, Yield14.8 MPa2140 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus1.06 GPa154 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus1.36 GPa197 ksi ASTM D790
Flexural Strength30.2 MPa4380 psi ASTM D790
Dart Drop Total Energy10.7 J/cm0.02 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy10.7 J/cm0.02 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.32 J/cm0.6 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.481 J/cm0.9 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.961 J/cm1.8 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F55.8 µm/m-°C31 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)56.1 °C133 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature182 - 193 °C360 - 380 °F Extrusion

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.