MatWeb, The Online Materials Database

PolyOne Geon® 87160 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • High Impact
  • UL 94 V0
  • UL 94 5VA
  • CSA V0
  • CSA 5VA
  • NSF STD 51

Applications:

  • General Purpose
  • Custom Profiles

Processing Method:

  • Extrusion-Single Screw

Disclaimer: Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.
Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.4 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D83.1 15 sec; ASTM D2240
Tensile Strength, Yield6340 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus419700 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus419 ksi ASTM D790
Flexural Strength11930 psi ASTM D790
Dart Drop Total Energy0.12 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.3 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched2 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched2.4 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F35.6 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)160 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0 All Colors; 0.03 in.
Flammability, UL947 All Colors; 0.059 in.

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178413354 ASTM D1784
Ease of SizingGood 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.