MatWeb, The Online Materials Database

PolyOne Geon® 87231 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Substrate for DURACAP

Applications:

  • Custom Profiles

Processing Method:

  • CoExtrusion

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.43 g/cc0.0517 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D81.681.6 15 sec; ASTM D2240
Tensile Strength, Yield48.2 MPa6990 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus3.03 GPa439 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus3 GPa435 ksi ASTM D790
Flexural Strength86.9 MPa12600 psi ASTM D790
Dart Drop Total Energy37.4 J/cm0.07 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy37.4 J/cm0.07 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched1.33 J/cm2.5 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched1.6 J/cm3 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F61.2 µm/m-°C34 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)73.9 °C165 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature182 - 193 °C360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178413354 ASTM D1784
Ease of SizingGood 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.