MatWeb, The Online Materials Database
PolyOne Geon® 87322 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - NSF Type II
- UL 94 V0
- High Impact
- Medium Flow
Market: - Building and Construction
Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.33 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.002 - 0.005 cm/cm | ASTM D955 |
Spiral Flow | 31 in | |
Mechanical Properties |
|
Hardness, Shore D | 83 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 6600 psi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Elongation at Break | 110 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 400000 psi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Flexural Modulus | 420 ksi | ASTM D790 |
Flexural Strength | 12000 psi | ASTM D790 |
Izod Impact, Notched | 1.6 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 0°F (-18°C); ASTM D256 |
Izod Impact, Notched | 20 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 162 °F | Unannealed, 0.250 in bars; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 172 °F | Annealed, 0.250 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 390 - 410 °F | Molding |
Descriptive Properties | |
Cell Classification D1784 | 16354 | ASTM D1784 |
NSF | Acceptable | Std 14-Plastic Piping Comp. |
NSF | Acceptable | Std 61-Drinking Water Appl. |
Product Form | Pellets/Cubes | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|