MatWeb, The Online Materials Database

PolyOne Geon® 87416 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior-Excellent Weatherability
  • High Impact
  • Broad Color Palette
  • UL 94 V0
  • CSA V0
  • CSA A440
  • AAMA 303

Applications:

  • Custom Profiles
  • Custom Profiles-Thin wall
  • Window Components

Market:

  • Windows
  • Automotive

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.45 g/cc0.0524 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D8282 15 sec; ASTM D2240
Tensile Strength, Yield44.1 MPa6400 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.48 GPa360 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.96 GPa430 ksi ASTM D790
Flexural Strength84.8 MPa12300 psi ASTM D790
Dart Drop Total Energy53.4 J/cm0.1 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy176 J/cm0.33 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched1.55 J/cm2.9 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched1.6 J/cm3 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched1.6 J/cm3 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F61.2 µm/m-°C34 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)72.8 °C163 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0V-0 All Colors; 0.03 in.
Flammability, UL94V-0V-0 All Colors; 0.039 in.

Processing Properties
Melt Temperature182 - 193 °C360 - 380 °F Extrusion

Descriptive Properties
AAMA 303Pass ASTM D4726
Automotive ApprovalGeneral Motors, GMP 7001M PVC 
Cell Classification D178413344 ASTM D1784
Cell Classification D421613143233 ASTM D4216
Ease of SizingAcceptable 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.