PolyOne Geon® 87416 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior-Excellent Weatherability
  • High Impact
  • Broad Color Palette
  • UL 94 V0
  • CSA V0
  • CSA A440
  • AAMA 303

Applications:

  • Custom Profiles
  • Custom Profiles-Thin wall
  • Window Components

Market:

  • Windows
  • Automotive

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.45 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D82 15 sec; ASTM D2240
Tensile Strength, Yield6400 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus360000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus430 ksi ASTM D790
Flexural Strength12300 psi ASTM D790
Dart Drop Total Energy0.1 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.33 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched2.9 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched3 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched3 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F34 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)163 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0 All Colors; 0.03 in.
Flammability, UL94V-0 All Colors; 0.039 in.

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
AAMA 303Pass ASTM D4726
Automotive ApprovalGeneral Motors, GMP 7001M PVC 
Cell Classification D178413344 ASTM D1784
Cell Classification D421613143233 ASTM D4216
Ease of SizingAcceptable 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.