PolyOne Geon® 87431 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • NSF Type I
  • PPI-2000 psi Rated
  • Normal Impact
  • Low Flow

Market:

  • Fittings (Potable Water, DWV, etc.)

Processing Method:

  • Injection Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.38 g/cc0.0499 lb/in³ ASTM D792
Linear Mold Shrinkage0.002 - 0.005 cm/cm0.002 - 0.005 in/in ASTM D955

Mechanical Properties
Hardness, Shore D8888 Instantaneous; ASTM D2240
Tensile Strength, Yield53.1 MPa7700 psi Type 1 - Rigids, 2 in/min; ASTM D638
Tensile Modulus3.07 GPa445 ksi Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Modulus3.31 GPa480 ksi ASTM D790
Flexural Strength93.8 MPa13600 psi ASTM D790
Izod Impact, Notched0.481 J/cm0.9 ft-lb/in Method A, Injection Molded, 0.250 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.534 J/cm1 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)72.2 °C162 °F Unannealed, 0.250 in bars; ASTM D648

Processing Properties
Melt Temperature202 - 204 °C395 - 400 °F Molding

Descriptive Properties
Cell Classification D178412464 ASTM D1784
NSFAcceptable Std 14-Plastic Piping Comp.
NSFAcceptable Std 61-Drinking Water Appl.
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.