MatWeb, The Online Materials Database

PolyOne Geon® 87624 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior UV Stable
  • Pearlescent Appearance
  • Dark Colors

Applications:

  • Custom Profiles
  • Capstock
  • Vertical Blinds

Processing Method:

  • CoExtrusion
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.39 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D84 15 sec; ASTM D2240
Tensile Strength, Yield7000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus400000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus500 ksi ASTM D790
Flexural Strength13000 psi ASTM D790
Dart Drop Total Energy0.09 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.17 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.6 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.6 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F36 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)149 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature360 - 390 °F Extrusion

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.