MatWeb, The Online Materials Database
PolyOne Geon® 87703 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: - Custom Profiles
- Window Components
Market: Processing Method: Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 84 | 84 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 43.6 MPa | 6320 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 3.28 GPa | 476 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 3.35 GPa | 486 ksi | ASTM D790 |
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Dart Drop Total Energy | 74.7 J/cm | 0.14 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 74.7 J/cm | 0.14 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 4.75 J/cm | 8.9 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
CTE, linear 68°F | 60.1 µm/m-°C | 33.4 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 73.9 °C | 165 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
Descriptive Properties | |
Cell Classification D4216 | 142234330101 | ASTM D4216 |
Ease of Sizing | Good | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|