MatWeb, The Online Materials Database

PolyOne Geon® 87703 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior-Weatherable

Applications:

  • Custom Profiles
  • Window Components

Market:

  • Windows

Processing Method:

  • Extrusion-Profile

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.49 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D84 15 sec; ASTM D2240
Tensile Strength, Yield6320 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus476000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus486 ksi ASTM D790
Flexural Strength13000 psi ASTM D790
Dart Drop Total Energy0.14 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.14 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched8.9 ft-lb/in Method A, Compression Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F33.4 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)165 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature360 - 390 °F 

Descriptive Properties
Cell Classification D4216142234330101 ASTM D4216
Ease of SizingGood 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.