PolyOne Geon® 87736 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Transparent
- Frosted Appearance
- Interior UV Stable
Applications: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.34 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore D | 82 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 7570 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 402600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 433 ksi | ASTM D790 |
| Flexural Strength | 13430 psi | ASTM D790 |
| Dart Drop Total Energy | 0.09 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Dart Drop Total Energy | 0.3 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Izod Impact, Notched | 1 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
| CTE, linear 68°F | 38 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 150 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 355 - 380 °F | Extrusion |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |