PolyOne Geon® 87759 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Low Smoke
  • UL 94 V0
  • ASTM E-84

Applications:

  • Custom Profiles

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.
Note: Finished part testing is required for ASTM E-84 certification.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.45 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D80 15 sec; ASTM D2240
Tensile Strength, Yield5890 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus420000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus393 ksi ASTM D790
Flexural Strength10100 psi ASTM D790
Dart Drop Total Energy0.1 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.12 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched3.5 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched3.7 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched4.3 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F39 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)154 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0 All Colors; 0.059 in.

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178413253 ASTM D1784
Ease of SizingGood 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.