Physical PropertiesOriginal ValueComments
Specific Gravity1.37 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D83 15 sec; ASTM D2240
Tensile Strength, Yield7360 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus398000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus412 ksi ASTM D790
Flexural Strength12900 psi ASTM D790
Dart Drop Total Energy0.11 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.32 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched15.7 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched18.8 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched26 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F35 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)154 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178416443 ASTM D1784
Ease of SizingAcceptable 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.