PolyOne Geon® 8800FR Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL Recognized Insulation per UL QMTT2
  • UL 105°C
  • Appliance Wiring Material of Extra High Quality
  • TW
  • THW
  • THHN
  • THWN
  • UL Oil Resistant II
  • Flame Retardant

Applications:

  • Telecommunication Insulation
  • Telecommunication Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.37 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D41 15 sec; ASTM D2240
Hardness, Shore D53 Instantaneous; ASTM D2240
Tensile Strength, Yield3500 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break300 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Modulus1800 psi Type 4 - Flexibles, 20 in/min; ASTM D638

Electrical Properties
Volume Resistivity1.8e+012 ohm-cm ASTM D257

Thermal Properties
Brittleness Temperature23 °F ASTM D746

Descriptive Properties
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.