MatWeb, The Online Materials Database

PolyOne Geon® 90004 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior
  • Low Gloss

Market:

  • Automotive

Processing Method:

  • Extrusion

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.32 g/cc ASTM D792
Collected Volatile Condensable Material0.31 % Method A, 221°F (105°C), 0.075 in; ASTM D1203B

Mechanical Properties
Hardness, Shore A92 15 sec; ASTM D2240
Tensile Strength, Ultimate3046 psi 20 in/min; ASTM D638
Elongation at Break325 % 20 in/min; ASTM D638
Tear Strength413 pli Die C (graves), 2 in/min; ASTM D1004

Descriptive Properties
Automotive ApprovalAftermarket Only, None 
Cold FlexibilityPass -22°F (-30°C), 25 mm, 4 hrs, 0.075 in; GM9503P
Fungal ResistancePass ASTM G21
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.