PolyOne Geon® 90005 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Low Gloss

Applications:

  • General Purpose
  • Protective Sleeves
  • Seat Welting

Market:

  • Automotive

Processing Method:

  • Extrusion

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.42 g/cc0.0513 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8888 15 sec; ASTM D2240
Tensile Strength, Ultimate10.3 MPa1494 psi 20 in/min, 100% in/in; ASTM D638
Tensile Strength, Ultimate16 MPa2321 psi 20 in/min; ASTM D638
Elongation at Break275 %275 % 20 in/min; ASTM D638
Tear Strength64 kN/m365 pli Die C (graves), 2 in/min; ASTM D1004

Thermal Properties
Brittleness Temperature-25 °C-13 °F ASTM D746

Descriptive Properties
Automotive ApprovalAftermarket Only, None 
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.