MatWeb, The Online Materials Database

PolyOne Geon® 90039 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior
  • Low Gloss

Applications:

  • Body Side Molding
  • Beltline Moldings
  • Greenhouse Trim

Market:

  • Automotive

Processing Method:

  • Extrusion
PolyOne First Choice

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.34 g/cc0.0484 lb/in³ ASTM D792
Collected Volatile Condensable Material0.29 %0.29 % Emery, 221°F (105°C), 0.075 in; ASTM D1203B

Mechanical Properties
Hardness, Shore A8686 15 sec; ASTM D2240
Tensile Strength, Ultimate19.2 MPa2785 psi 20 in/min; ASTM D638
Elongation at Break320 %320 % 20 in/min; ASTM D638
Tear Strength66.3 kN/m378 pli Die C (graves), 2 in/min; ASTM D1004

Descriptive Properties
Automotive ApprovalGeneral Motors, GMP.PVC.010 
Fungal ResistancePass ASTM G21
Low Temperature Flexibility (LTF)Pass 12 mm, -20°F (-29°C), 4 hrs, 0.020 in
Product FormPellets 
Xenon Weatherometer - ExteriorPass 2,500 kJ/m², Black, dE*; SAE J1960

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.