PolyOne Geon® 90048 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior
  • High Gloss
  • Transparent

Applications:

  • Body Side Molding

Market:

  • Automotive

Processing Method:

  • Extrusion
  • CoExtrusion
PolyOne First Choice

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.25 g/cc0.0452 lb/in³ ASTM D792
Collected Volatile Condensable Material0.4 %0.4 % Method A, 221°F (105°C), 0.075 in; ASTM D1203B

Mechanical Properties
Hardness, Shore D3737 15 sec; ASTM D2240
Tensile Strength, Ultimate22 MPa3191 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break285 %285 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength70.1 kN/m400 pli Die C (graves), 2 in/min; ASTM D1004

Descriptive Properties
Automotive ApprovalGeneral Motors, GMP.PVC.003 Pass
Fungal ResistancePass ASTM G21
Low Temperature Flexibility (LTF)Pass 12 mm, -20°F (-29°C), 4 hrs, 0.020 in
Product FormPellets 
Xenon Weatherometer - ExteriorPass 2,500 kJ/m², Natural, dE*; SAE J1960

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.