MatWeb, The Online Materials Database
PolyOne Geon® 90049 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior
- High Gloss
- Transparent
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
| Collected Volatile Condensable Material | 0.43 % | 0.43 % | Emery, 221°F (105°C), 0.075 in; ASTM D1203B |
Mechanical Properties |
|
| Hardness, Shore A | 83 | 83 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 19.2 MPa | 2785 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 324 % | 324 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 63.3 kN/m | 361 pli | Die C (graves), 2 in/min; ASTM D1004 |
Descriptive Properties | |
| Automotive Approval | General Motors, GMP.PVC.010 | Pass |
| Automotive Approval | DaimlerChrysler, MS-DC211-B | Pass |
| Fungal Resistance | Pass | ASTM G21 |
| Low Temperature Flexibility (LTF) | Pass | 12 mm, -20°F (-29°C), 4 hrs, 0.020 in |
| Product Form | Pellets | |
| Xenon Weatherometer - Exterior | Pass | 2,500 kJ/m², Natural, dE*; SAE J1960 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |