PolyOne Geon® 90072 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • High Gloss
  • Transparent

Market:

  • Automotive
  • Recreational

Processing Method:

  • Extrusion
  • CoExtrusion
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.26 g/cc0.0455 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8888 15 sec; ASTM D2240
Tensile Strength, Ultimate19.5 MPa2828 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break260 %260 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength87.7 kN/m500 pli Die C (graves), 2 in/min; ASTM D1004

Thermal Properties
Brittleness Temperature-28 °C-18.4 °F ASTM D746

Processing Properties
Melt Temperature177 - 188 °C350 - 370 °F 

Descriptive Properties
Automotive ApprovalAftermarket Only, None 
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.