PolyOne Geon® 90100 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Transparent
  • High Gloss
  • Low Migration

Applications:

  • Hose and Tubing
  • Windshield Washer Tubing

Market:

  • Automotive
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.22 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A71 15 sec; ASTM D2240
Tensile Strength, Ultimate2050 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break340 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Flammability Test0.6 in/min; FMVSS 302

Processing Properties
Melt Temperature340 - 360 °F Extrusion

Descriptive Properties
Automotive ApprovalHonda, HES B 045-89 Pass
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.