MatWeb, The Online Materials Database

PolyOne Geon® 90206 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • General Purpose Grade

Applications:

  • Seat Welting
  • Protective Sleeves

Market:

  • Automotive - Aftermarket

Processing Method:

  • Extrusion and Molding

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.39 g/cc0.0502 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8484 15 sec; ASTM D2240
Hardness, Shore A9090 Instantaneous; ASTM D2240
Tensile Strength, Ultimate16.8 MPa2437 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break330 %330 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength64 kN/m365 pli Die C (graves), 2 in/min; ASTM D1004

Thermal Properties
Brittleness Temperature-24 °C-11.2 °F ASTM D746
Flammability Test00 in/min; FMVSS 302

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.