MatWeb, The Online Materials Database

PolyOne Geon® 90251 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • General Purpose Grade

Applications:

  • Protective Sleeves
  • Gaskets and Seals

Market:

  • Automotive - Aftermarket

Processing Method:

  • Extrusion and Molding

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.26 g/cc0.0455 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A7070 15 sec; ASTM D2240
Hardness, Shore A7878 Instantaneous; ASTM D2240
Tensile Strength, Ultimate13 MPa1885 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Strength, Ultimate5.3 MPa769 psi Type 4 - Flexibles, 20 in/min, 100% in/in; ASTM D638
Elongation at Break430 %430 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength42.1 kN/m240 pli Die C (graves), 2 in/min; ASTM D1004

Thermal Properties
Brittleness Temperature-42 °C-43.6 °F ASTM D746

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.