MatWeb, The Online Materials Database

PolyOne Geon® 90401 Vinyl Alloy - Flexible (FPVC alloy)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Low Gloss

Applications:

  • Arm Rest
  • Head Rest

Market:

  • Automotive

Processing Method:

  • Blow Molding

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.24 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A75 15 sec; ASTM D2240
Tensile Strength, Ultimate2060 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break313 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength206 pli Die C (graves), 20 in/min; ASTM D624

Thermal Properties
Flammability Test0 in/min; FMVSS 302

Optical Properties
Gloss3.5 % 60º Gardner; ASTM D523

Descriptive Properties
Automotive ApprovalGeneral Motors, GMP.PVC.077 
Cold FlexibilityPass -20°F (-29°C), 25 mm, 4 hrs, 0.075 in; GM9503P
Fogging86 % 3 hrs, 212°F (100°C), 70°F (21°C), after 1 hour; SAE J1756
Product FormPellets 
Xenon Weatherometer - InteriorPass 1,240 kJ/m², All Colors, dE*; SAE J1885

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.