Physical PropertiesOriginal ValueComments
Specific Gravity1.28 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A57 15 sec; ASTM D2240
Tensile Strength, Ultimate1711 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break400 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength233 pli Die C (graves), 20 in/min; ASTM D624

Thermal Properties
Flammability Test0 in/min; FMVSS 302

Descriptive Properties
Automotive ApprovalFord, WSK M4D 871 A1 
Cold FlexibilityPass -20°F (-29°C), 25 mm, 4 hrs, 0.075 in; GM9503P
Fogging86 % 3 hrs, 212°F (100°C), 70°F (21°C), after 1 hour; SAE J1756
Product FormPellets 
Xenon Weatherometer - InteriorPass 1,240 kJ/m², All Colors, dE*; SAE J1885

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.