MatWeb, The Online Materials Database
PolyOne Geon® 90451 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 72 | 72 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 13.4 MPa | 1940 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 345 % | 345 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 56.1 kN/m | 320 pli | Die C (graves), 20 in/min; ASTM D624 |
Thermal Properties |
|
| Brittleness Temperature | -34 °C | -29.2 °F | ASTM D746 |
| Flammability Test | 0 | 0 | in/min; FMVSS 302 |
Descriptive Properties | |
| Automotive Approval | Subaru, None | |
| Cold Flexibility | Pass | -20°F (-29°C), 25 mm, 4 hrs, 0.075 in; GM9503P |
| Fogging | 90 % | 3 hrs, 212°F (100°C), 70°F (21°C), after 1 hour; SAE J1756 |
| Fogging | 88 % | 6 hrs, 203°F (95°C), 100°F (38°C), after 16 hours; SAE J1756 |
| Product Form | Pellets | |
| Xenon Weatherometer - Interior | Pass | 602 kj/m², All Colors, dE*; SAE J1885 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of