MatWeb, The Online Materials Database

Degussa AG VESTAMID® L1621 sw (dry properties) Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Uses: Cable ties, strip clips.

Physical PropertiesMetricEnglishComments
Density1.03 g/cc0.0372 lb/in³ 
Moisture Absorption at EquilibriumMax 0.5 %Max 0.5 % Humidity Absorption
Melt Flow190 g/10 min190 g/10 min 

Mechanical Properties
Tensile Strength, Yield33 MPa4790 psi 
Elongation at BreakMin 50 %Min 50 % 
Elongation at Yield23 %23 % 
Modulus of Elasticity0.65 GPa94.3 ksi 
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.7 J/cm²3.33 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB at -30°C
Charpy Impact, Notched1.3 J/cm²6.19 ft-lb/in² 

Electrical Properties
Electrical Resistivity2e+013 ohm-cm2e+013 ohm-cm 
Surface ResistanceMin 1e+015 ohmMin 1e+015 ohm 
Dielectric Constant33 at 1 MHz.
Dielectric Constant, Low Frequency77 100 Hz
Dielectric Strength32 kV/mm813 kV/in 
Dissipation Factor0.0750.075 at 1 MHz.
Dissipation Factor, Low Frequency0.140.14 100 Hz
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F in flow direction.
CTE, linear 20°C Transverse to Flow100 µm/m-°C55.6 µin/in-°F 
Deflection Temperature at 0.46 MPa (66 psi)110 °C230 °F 
Deflection Temperature at 1.8 MPa (264 psi)45 °C113 °F 
Vicat Softening Point140 °C284 °F 50°C/hr/50 N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94HBHB 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.