MatWeb, The Online Materials Database

Degussa AG VESTAMID® L1640 nf (as-conditioned) Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Uses: Wire insulation, fiber optics jacketing.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ 
Moisture Absorption at EquilibriumMax 0.5 %Max 0.5 % Humidity Absorption

Mechanical Properties
Tensile Strength, Yield38 MPa5510 psi 
Elongation at BreakMin 50 %Min 50 % 
Elongation at Yield9 %9 % 
Modulus of Elasticity1.2 GPa174 ksi 
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.4 J/cm²1.9 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB at -30°C
Charpy Impact, Notched0.4 J/cm²1.9 ft-lb/in² 

Electrical Properties
Electrical Resistivity4e+014 ohm-cm4e+014 ohm-cm 
Surface ResistanceMin 1e+015 ohmMin 1e+015 ohm 
Dielectric Constant33 at 1 MHz.
Dielectric Constant, Low Frequency55 100 Hz
Dielectric Strength30 kV/mm762 kV/in 
Dissipation Factor0.050.05 at 1 MHz.
Dissipation Factor, Low Frequency0.0750.075 100 Hz

Thermal Properties
CTE, linear 20°CMax 50 µm/m-°CMax 27.8 µin/in-°F 
Deflection Temperature at 0.46 MPa (66 psi)110 °C230 °F 
Deflection Temperature at 1.8 MPa (264 psi)45 °C113 °F 
Vicat Softening Point140 °C284 °F 50°C/hr/50 N
UL RTI, Electrical110 °C230 °F 
UL RTI, Mechanical with Impact70 °C158 °F 
UL RTI, Mechanical without Impact95 °C203 °F 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.