MatWeb, The Online Materials Database

Degussa AG VESTAMID® L2140 sw 9.7504 (dry properties) Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Uses: Tubing for the automobile industry according to DIN 73 378, Type: PA 12-HL.

Physical PropertiesOriginal ValueComments
Density1.01 g/cc 
Water Absorption1 % 
Moisture Absorption at EquilibriumMax 0.5 % Humidity Absorption
Melt Flow30 g/10 min 

Mechanical Properties
Tensile Strength, Yield48 MPa 
Elongation at BreakMin 50 % 
Elongation at Yield5 % 
Modulus of Elasticity1.5 GPa 
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.7 J/cm² at -30°C
Charpy Impact, Unnotched Low TempNB at -30°C
Charpy Impact, Notched1.1 J/cm² 

Electrical Properties
Electrical Resistivity2e+014 ohm-cm 
Surface ResistanceMin 1e+015 ohm 
Dielectric Constant3 at 1 MHz.
Dielectric Constant, Low Frequency3 100 Hz
Dielectric Strength32 kV/mm 
Dissipation Factor0.03 at 1 MHz.
Dissipation Factor, Low Frequency0.04 100 Hz
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C in flow direction.
CTE, linear 20°C Transverse to Flow100 µm/m-°C 
Deflection Temperature at 0.46 MPa (66 psi)110 °C 
Deflection Temperature at 1.8 MPa (264 psi)50 °C 
Vicat Softening Point140 °C 50°C/hr/50 N
UL RTI, Electrical120 °C 
UL RTI, Mechanical with Impact85 °C 
UL RTI, Mechanical without Impact95 °C 
Flammability, UL94HB 1.6 mm
Flammability, UL94HB 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.