Degussa AG VESTAMID® L2140 sw 9.7504 (as-conditioned) Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Uses: Tubing for the automobile industry according to DIN 73 378, Type: PA 12-HL.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ 
Moisture Absorption at EquilibriumMax 0.5 %Max 0.5 % Humidity Absorption

Mechanical Properties
Tensile Strength, Yield41 MPa5950 psi 
Elongation at BreakMin 50 %Min 50 % 
Elongation at Yield13 %13 % 
Modulus of Elasticity1.3 GPa189 ksi 
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp1 J/cm²4.76 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB at -30°C
Charpy Impact, Notched1.2 J/cm²5.71 ft-lb/in² 

Electrical Properties
Electrical Resistivity3e+014 ohm-cm3e+014 ohm-cm 
Surface ResistanceMin 1e+015 ohmMin 1e+015 ohm 
Dielectric Constant33 at 1 MHz.
Dielectric Constant, Low Frequency44 100 Hz
Dielectric Strength35 kV/mm889 kV/in 
Dissipation Factor0.050.05 at 1 MHz.
Dissipation Factor, Low Frequency0.070.07 100 Hz

Thermal Properties
CTE, linear 20°CMax 50 µm/m-°CMax 27.8 µin/in-°F 
Vicat Softening Point140 °C284 °F 50°C/hr/50 N
UL RTI, Electrical120 °C248 °F 
UL RTI, Mechanical with Impact85 °C185 °F 
UL RTI, Mechanical without Impact95 °C203 °F 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.