Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ 
Water Absorption1 %1 % 
Moisture Absorption at EquilibriumMax 0.5 %Max 0.5 % Humidity Absorption
Melt Flow36 g/10 min36 g/10 min 

Mechanical Properties
Tensile Strength, Yield47 MPa6820 psi 
Elongation at BreakMin 50 %Min 50 % 
Elongation at Yield5 %5 % 
Modulus of Elasticity1.5 GPa218 ksi 
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.9 J/cm²4.28 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB at -30°C
Charpy Impact, Notched1.6 J/cm²7.61 ft-lb/in² 

Electrical Properties
Electrical ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm 
Surface ResistanceMin 1e+015 ohmMin 1e+015 ohm 
Dielectric Constant33 at 1 MHz.
Dielectric Constant, Low Frequency33 100 Hz
Dielectric Strength26 kV/mm660 kV/in 
Dissipation Factor0.0260.026 at 1 MHz.
Dissipation Factor, Low Frequency0.0390.039 100 Hz
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F in flow direction.
CTE, linear 20°C Transverse to Flow100 µm/m-°C55.6 µin/in-°F 
Deflection Temperature at 0.46 MPa (66 psi)110 °C230 °F 
Deflection Temperature at 1.8 MPa (264 psi)50 °C122 °F 
Vicat Softening Point140 °C284 °F 50°C/hr/50 N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94HBHB 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.