Physical PropertiesOriginal ValueComments
Density1.01 g/cc 

Mechanical Properties
Hardness, Shore D66 
Tensile Strength, Yield27 MPa 
Elongation at BreakMin 50 % 
Elongation at Yield25 % 
Modulus of Elasticity0.53 GPa 
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.9 J/cm² at -30°C
Charpy Impact, Unnotched Low TempNB at -30°C
Charpy Impact, NotchedNB 

Electrical Properties
Electrical Resistivity7e+012 ohm-cm 
Dielectric Constant4 at 1 MHz.
Dielectric Constant, Low Frequency9 100 Hz
Dielectric Strength32 kV/mm 
Dissipation Factor0.11 at 1 MHz.
Dissipation Factor, Low Frequency0.14 100 Hz
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C in flow direction.
CTE, linear 20°C Transverse to Flow100 µm/m-°C 
Deflection Temperature at 0.46 MPa (66 psi)100 °C 
Deflection Temperature at 1.8 MPa (264 psi)45 °C 
Vicat Softening Point130 °C 50°C/hr/50 N
Flammability, UL94HB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.