MatWeb, The Online Materials Database

Degussa AG VESTAMID® X7325 nf (dry properties) Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Physical PropertiesMetricEnglishComments
Density1.96 g/cc0.0708 lb/in³ 

Mechanical Properties
Tensile Strength, Yield90 MPa13100 psi 
Elongation at Break6 %6 % 
Elongation at Yield3 %3 % 
Modulus of Elasticity8 GPa1160 ksi 
Charpy Impact Unnotched5 J/cm²23.8 ft-lb/in² 
Charpy Impact, Notched, Low Temp0.9 J/cm²4.28 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp5 J/cm²23.8 ft-lb/in² at -30°C
Charpy Impact, Notched1.1 J/cm²5.24 ft-lb/in² 

Electrical Properties
Electrical Resistivity6e+014 ohm-cm6e+014 ohm-cm 
Surface ResistanceMin 1e+015 ohmMin 1e+015 ohm 
Dielectric Constant44 at 1 MHz.
Dielectric Constant, Low Frequency44 100 Hz
Dissipation Factor0.0380.038 at 1 MHz.
Dissipation Factor, Low Frequency0.0550.055 100 Hz
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°CMax 50 µm/m-°CMax 27.8 µin/in-°F Parallel direction
CTE, linear 20°C Transverse to FlowMax 50 µm/m-°CMax 27.8 µin/in-°F 
Deflection Temperature at 0.46 MPa (66 psi)175 °C347 °F 
Deflection Temperature at 1.8 MPa (264 psi)160 °C320 °F 
Vicat Softening Point170 °C338 °F 50°C/hr/50 N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94HBHB 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.