Degussa AG VESTAMID® X7375 nf (dry properties) Polyether Block Amide (PEBA)
Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Polymer; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Uses: Ski upper surfaces.
Physical Properties | Metric | English | Comments |
|
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Water Absorption | 1 % | 1 % | |
Mechanical Properties |
|
Hardness, Shore D | 68 | 68 | |
Tensile Strength, Yield | 31 MPa | 4500 psi | |
Elongation at Break | Min 50 % | Min 50 % | |
Elongation at Yield | 19 % | 19 % | |
Modulus of Elasticity | 0.75 GPa | 109 ksi | |
Charpy Impact Unnotched | NB | NB | |
Charpy Impact, Notched, Low Temp | 0.7 J/cm² | 3.33 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | NB | at -30°C |
Charpy Impact, Notched | 4.4 J/cm² | 20.9 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | 2e+013 ohm-cm | 2e+013 ohm-cm | |
Dielectric Constant | 4 | 4 | at 1 MHz. |
Dielectric Constant, Low Frequency | 7 | 7 | 100 Hz |
Dielectric Strength | 30 kV/mm | 762 kV/in | |
Dissipation Factor | 0.076 | 0.076 | at 1 MHz. |
Dissipation Factor, Low Frequency | 0.15 | 0.15 | 100 Hz |
Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 100 µm/m-°C | 55.6 µin/in-°F | in flow direction. |
CTE, linear 20°C Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Deflection Temperature at 0.46 MPa (66 psi) | 100 °C | 212 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 45 °C | 113 °F | |
Vicat Softening Point | 130 °C | 266 °F | 50°C/hr/50 N |
Flammability, UL94 | HB | HB | 1.6 mm |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|