Degussa AG Vestamid® D18 Nylon 612 (Conditioned)


Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic

Key Words: PA612, LN, 14-020

Material Notes:
Description: medium-viscosity base product

Applications: monofilaments, bristles with high recovery for paint brushes and tooth brushes

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.06 g/cc0.0383 lb/in³ ISO 1183

Mechanical Properties
Tensile Strength, Yield52 MPa7540 psi ISO 527-2/1A
Elongation at BreakMin 50 %Min 50 % ISO 527-2/1A
Elongation at Yield20 %20 % ISO 527-2/1A
Tensile Modulus1.7 GPa247 ksi ISO 527-2/1A
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.7 J/cm²3.33 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, Notched0.9 J/cm²4.28 ft-lb/in² 23°C; ISO 179/1eA

Thermal Properties
Melting Point215 °C419 °F Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)170 °C338 °F When conditioned at 180°C for 1 hour; ISO 75
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)75 °C167 °F When conditioned at 180°C for 1 hour; ISO 75
Vicat Softening Point180 °C356 °F 50N; ISO 306
Flammability, UL94HBHB 3.2 mm
Flammability, UL94HBHB 1.6 mm

Descriptive Properties
Electrolytic CorrosionA1 Step IEC 60426

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.