Degussa AG Vestamid® DX9320 Black 10% Glass Reinforced Nylon 612 (Conditioned)
 Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 612; Polymer; Thermoplastic 
Key Words: PA612-HI, MH, 14-040, GF10 
Material Notes:  Description:  impact-resistant, 10% glass fiber reinforced, medium-viscosity, heat-stabilized Applications: housings subject to impact, coverings with molded-on elastomer seals Information provided by degussa. 
| Physical Properties | Metric | English | Comments |  
 |  
| Density | 1.12 g/cc | 0.0405 lb/in³ |  ISO 1183 |  
 Mechanical Properties |  
 |  
| Tensile Strength at Break | 62 MPa | 8990 psi |  ISO 527-2/1A |  
| Tensile Strength, Yield | 67 MPa | 9720 psi |  ISO 527-2/1A |  
| Elongation at Break | 12 % | 12 % |  ISO 527-2/1A |  
| Elongation at Yield | 5 % | 5 % |  ISO 527-2/1A |  
| Tensile Modulus | 3.1 GPa | 450 ksi |  ISO 527-2/1A |  
| Charpy Impact Unnotched | 8.5 J/cm² | 40.5 ft-lb/in² |  23°C; ISO 179/1eU |  
| Charpy Impact, Notched, Low Temp | 0.5 J/cm² | 2.38 ft-lb/in² |  -30°C; ISO 179/1eA |  
| Charpy Impact, Unnotched Low Temp | 8.4 J/cm² | 40 ft-lb/in² |  -30°C; ISO 179/1eU |  
| Charpy Impact, Notched | 1.2 J/cm² | 5.71 ft-lb/in² |  23°C; ISO 179/1eA |  
 Thermal Properties |  
 |  
| Melting Point | 215 °C | 419 °F |  Peak Temperature; ISO 11357 |  
| Deflection Temperature at 0.46 MPa (66 psi) | 201 °C | 394 °F |  ISO 75 |  
| Deflection Temperature at 1.8 MPa (264 psi) | 183 °C | 361 °F |  ISO 75 |  
| Vicat Softening Point | 199 °C | 390 °F |  50N; ISO 306 |  
| Flammability, UL94 | HB | HB |  1.6 mm |  
 
	 | 
	  | 
	  | 
	
		
  
		Copyright 1996-2010 by Automation Creations, Inc.  The information provided by 
		MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not 
		be reproduced either electronically, photographically or substantively without permission from 
		Automation Creations, Inc.  No warranty, neither expressed nor implied, is given 
		regarding the accuracy of this information.  The user assumes all risk and liability in connection with the use of 
		information from MatWeb.
		
	 | 
	  |