| Physical Properties | Metric | English | Comments |
|
| Density | 1.19 g/cc | 0.043 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.8 % | 0.8 % | 23°C/50% R.H.; ISO 62 |
| Water Absorption at Saturation | 2 % | 2 % | ISO 62 |
| Linear Mold Shrinkage | 0.0066 cm/cm | 0.0066 in/in | 127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2) |
| Linear Mold Shrinkage, Transverse | 0.0088 cm/cm | 0.0088 in/in | 127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2) |
Mechanical Properties |
|
| Tensile Strength at Break | 109 MPa | 15800 psi | ISO 527-2/1A |
| Elongation at Break | 6 % | 6 % | ISO 527-2/1A |
| Tensile Modulus | 5.45 GPa | 790 ksi | ISO 527-2/1A |
| Charpy Impact Unnotched | 9.3 J/cm² | 44.3 ft-lb/in² | 23°C; ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 1.1 J/cm² | 5.24 ft-lb/in² | -30°C; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | 10.6 J/cm² | 50.4 ft-lb/in² | -30°C; ISO 179/1eU |
| Charpy Impact, Notched | 1.8 J/cm² | 8.57 ft-lb/in² | 23°C; ISO 179/1eA |
Electrical Properties |
|
| Volume Resistivity | 1e+014 ohm-cm | 1e+014 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.1 | 3.1 | 23°C/1 MHz; IEC 60250 |
| Dielectric Constant, Low Frequency | 4.4 | 4.4 | 23°C/100 Hz; IEC 60250 |
| Dissipation Factor | 0.047 | 0.047 | 23°C/1 MHz; IEC 60250 |
| Dissipation Factor, Low Frequency | 0.05 | 0.05 | 23°C/100 Hz; IEC 60250 |
| Comparative Tracking Index | Min 600 V | Min 600 V | Test Solution A, 50 drops; IEC 60112 |
| Comparative Tracking Index | 600 V | 600 V | Test Solution A, 100 drops; IEC 60112 |
Thermal Properties |
|
| CTE, linear 20°C | 50 µm/m-°C | 27.8 µin/in-°F | 23-55°C, Longitudinal; ISO 11359 |
| CTE, linear 20°C | 70 µm/m-°C | 38.9 µin/in-°F | 23-55°C, Transverse; ISO 11359 |
| Melting Point | 215 °C | 419 °F | Peak Temperature; ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 208 °C | 406 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 189 °C | 372 °F | ISO 75 |
| Vicat Softening Point | 207 °C | 405 °F | 50N; ISO 306 |
| Flammability, UL94 | HB | HB | 1.6 mm |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |