MatWeb, The Online Materials Database

Degussa AG Vestamid® E47-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer


Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic

Material Notes:
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:

  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: sports shoe soles, packaging films, non-skid surfaces, sports glasses, protective goggles

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.02 g/cc0.0368 lb/in³ ISO 1183
Water Absorption at Saturation1 %1 % ISO 62
Viscosity Test190 cm³/g190 cm³/g Viscosity Number; ISO 307
Linear Mold Shrinkage0.006 - 0.01 cm/cm0.006 - 0.01 in/in 3 mm sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse0.009 - 0.015 cm/cm0.009 - 0.015 in/in 3 mm sheet with film gate at rim, mold temperature 80°C

Mechanical Properties
Hardness, Shore D4747 ISO 868
Tensile Strength at Break23 MPa3340 psi ISO 527-1, ISO 527-2
Elongation at BreakMin 200 %Min 200 % ISO 527-1, ISO 527-2
Tensile Modulus0.12 GPa17.4 ksi ISO 527-1, ISO 527-2
50% Modulus0.012 GPa1.74 ksi ISO 527-1, ISO 527-2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low TempNBNB -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, NotchedNBNB 23°C; ISO 179/1eA
Tensile Creep Modulus, 1000 hours90 MPa13100 psi ISO 899-1

Electrical Properties
Volume Resistivity1e+011 ohm-cm1e+011 ohm-cm Spec.; IEC 60093
Surface Resistance1e+013 ohm1e+013 ohm Spec.; IEC 60093
Dielectric Constant4.74.7 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency8.58.5 23°C/100 Hz; IEC 60250
Dielectric Strength37 kV/mm940 kV/in K20/P50; IEC 60243-1
Dissipation Factor0.130.13 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.120.12 23°C/100 Hz; IEC 60250
Comparative Tracking Index600 V600 V Test Solution A; IEC 60112

Thermal Properties
CTE, linear 20°C210 µm/m-°C117 µin/in-°F 23-55°C, Transverse; ISO 11359
CTE, linear 20°C230 µm/m-°C128 µin/in-°F 23-55°C, Longitudinal; ISO 11359
Deflection Temperature at 0.46 MPa (66 psi)65 °C149 °F ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi)45 °C113 °F ISO 75-1
Vicat Softening Point140 °C284 °F 10N; ISO 306
Vicat Softening Point70 °C158 °F 50N; ISO 306
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.