Degussa AG Vestamid® E50-R2 Heat & Light Stabilized Nylon 12/PEBA Elastomer


Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic

Material Notes:
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:

  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: permanently antistatic articles (R=102 - 105?), e.g., conveyor belts, housings, paint spray hoses

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.08 g/cc0.039 lb/in³ ISO 1183

Mechanical Properties
Hardness, Shore D5050 ISO 868
Tensile Strength at Break20 MPa2900 psi ISO 527-1, ISO 527-2
Elongation at BreakMin 200 %Min 200 % ISO 527-1, ISO 527-2
Tensile Modulus0.17 GPa24.7 ksi ISO 527-1, ISO 527-2
50% Modulus0.013 GPa1.89 ksi ISO 527-1, ISO 527-2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low TempNBNB -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, NotchedNBNB 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1000 ohm-cm1000 ohm-cm Spec.; IEC 60093
Surface Resistance10000 ohm10000 ohm Spec.; IEC 60093

Thermal Properties
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.