MatWeb, The Online Materials Database
Degussa AG Vestamid® E50-R2 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic
Material Notes: Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:- They have low density.
- They are highly resistant to chemicals and solvents.
- They are easy to process and color and are easy to overmold.
- They can be decorated easily by means of heat transfer printing.
- They have excellent impact strength at low temperatures.
- Their hardness and flexibility can be varied over a wide range.
- They have high elasticity and good recovery.
- Their mechanical properties are only slightly temperature-dependent.
- They are free of volatile or migrating plasticizers.
Applications: permanently antistatic articles (R=102 - 105?), e.g., conveyor belts, housings, paint spray hoses Information provided by degussa.
Physical Properties | Original Value | Comments |
|
Density | 1.08 g/cc | ISO 1183 |
Mechanical Properties |
|
Hardness, Shore D | 50 | ISO 868 |
Tensile Strength at Break | 20 MPa | ISO 527-1, ISO 527-2 |
Elongation at Break | Min 200 % | ISO 527-1, ISO 527-2 |
Tensile Modulus | 0.17 GPa | ISO 527-1, ISO 527-2 |
50% Modulus | 0.013 GPa | ISO 527-1, ISO 527-2 |
Charpy Impact Unnotched | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | NB | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | -30°C; ISO 179/1eU |
Charpy Impact, Notched | NB | 23°C; ISO 179/1eA |
Electrical Properties |
|
Volume Resistivity | 1000 ohm-cm | Spec.; IEC 60093 |
Surface Resistance | 10000 ohm | Spec.; IEC 60093 |
Thermal Properties |
|
Flammability, UL94 | HB | 1.6 mm |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|