MatWeb, The Online Materials Database

Degussa AG Vestamid® E62-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer for Fiber Optic Jacketing


Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic

Material Notes:
Description: E62-S3 is a PA 12 block copolymer consisting of PA 12 segments and polyether segments. The compound exhibits high flexibility and high chemical and solvent resistance.

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ ISO 1183
Water Absorption at Saturation1.5 %1.5 % ISO 62
Melt Flow20.2 g/10 min20.2 g/10 min 250°C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Shore D6262 ISO 868
Tensile Strength, Yield24 MPa3480 psi ISO 527-2/1A
Elongation at BreakMin 50 %Min 50 % ISO 527-2/1A
Elongation at Yield31 %31 % ISO 527-2/1A
Tensile Modulus0.36 GPa52.2 ksi ISO 527-1/2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.8 J/cm²3.81 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, Notched12 J/cm²57.1 ft-lb/in² 23°C, Partial Break; ISO 179/1eA

Thermal Properties
CTE, linear 20°C200 µm/m-°C111 µin/in-°F 23-80°C; ISO 11359
Melting Point175 - 178 °C347 - 352 °F DSC

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.