MatWeb, The Online Materials Database
Degussa AG Vestamid® EX9200 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic
Material Notes: Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:- They have low density.
- They are highly resistant to chemicals and solvents.
- They are easy to process and color and are easy to overmold.
- They can be decorated easily by means of heat transfer printing.
- They have excellent impact strength at low temperatures.
- Their hardness and flexibility can be varied over a wide range.
- They have high elasticity and good recovery.
- Their mechanical properties are only slightly temperature-dependent.
- They are free of volatile or migrating plasticizers.
Applications: decorative and protective films for sports articles and interior/exterior designs on automobiles Information provided by degussa.
Physical Properties | Metric | English | Comments |
|
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Water Absorption at Saturation | 1.5 % | 1.5 % | ISO 62 |
Viscosity Test | 190 cm³/g | 190 cm³/g | Viscosity Number; ISO 307 |
Mechanical Properties |
|
Hardness, Shore D | 68 | 68 | ISO 868 |
Tensile Strength, Yield | 31 MPa | 4500 psi | ISO 527-1, ISO 527-2 |
Elongation at Break | Min 200 % | Min 200 % | ISO 527-1, ISO 527-2 |
Elongation at Yield | 19 % | 19 % | ISO 527-1, ISO 527-2 |
Tensile Modulus | 0.7 GPa | 102 ksi | ISO 527-1, ISO 527-2 |
50% Modulus | 0.027 GPa | 3.92 ksi | ISO 527-1, ISO 527-2 |
Charpy Impact Unnotched | NB | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.6 J/cm² | 2.86 ft-lb/in² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | NB | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 3.3 J/cm² | 15.7 ft-lb/in² | 23°C, Partial Break; ISO 179/1eA |
Electrical Properties |
|
Volume Resistivity | 1e+011 ohm-cm | 1e+011 ohm-cm | Spec.; IEC 60093 |
Surface Resistance | 1e+013 ohm | 1e+013 ohm | Spec.; IEC 60093 |
Dielectric Constant | 4.6 | 4.6 | 23°C/1 MHz; IEC 60250 |
Dielectric Constant, Low Frequency | 7.4 | 7.4 | 23°C/100 Hz; IEC 60250 |
Dielectric Strength | 30 kV/mm | 762 kV/in | K20/P50; IEC 60243-1 |
Dissipation Factor | 0.076 | 0.076 | 23°C/1 MHz; IEC 60250 |
Dissipation Factor, Low Frequency | 0.15 | 0.15 | 23°C/100 Hz; IEC 60250 |
Comparative Tracking Index | 600 V | 600 V | Test Solution A; IEC 60112 |
Thermal Properties |
|
CTE, linear 20°C | 160 µm/m-°C | 88.9 µin/in-°F | 23-55°C, Longitudinal; ISO 11359 |
CTE, linear 20°C | 160 µm/m-°C | 88.9 µin/in-°F | 23-55°C, Transverse; ISO 11359 |
Deflection Temperature at 0.46 MPa (66 psi) | 100 °C | 212 °F | ISO 75-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 45 °C | 113 °F | ISO 75-1 |
Vicat Softening Point | 130 °C | 266 °F | 50N; ISO 306 |
Vicat Softening Point | 170 °C | 338 °F | 10N; ISO 306 |
Flammability, UL94 | HB | HB | 1.6 mm |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|