Degussa AG Vestamid® EX9200 Heat & Light Stabilized Nylon 12/PEBA Elastomer


Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic

Material Notes:
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:

  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: decorative and protective films for sports articles and interior/exterior designs on automobiles

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.01 g/cc ISO 1183
Water Absorption at Saturation1.5 % ISO 62
Viscosity Test190 cm³/g Viscosity Number; ISO 307

Mechanical Properties
Hardness, Shore D68 ISO 868
Tensile Strength, Yield31 MPa ISO 527-1, ISO 527-2
Elongation at BreakMin 200 % ISO 527-1, ISO 527-2
Elongation at Yield19 % ISO 527-1, ISO 527-2
Tensile Modulus0.7 GPa ISO 527-1, ISO 527-2
50% Modulus0.027 GPa ISO 527-1, ISO 527-2
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.6 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched3.3 J/cm² 23°C, Partial Break; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+011 ohm-cm Spec.; IEC 60093
Surface Resistance1e+013 ohm Spec.; IEC 60093
Dielectric Constant4.6 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency7.4 23°C/100 Hz; IEC 60250
Dielectric Strength30 kV/mm K20/P50; IEC 60243-1
Dissipation Factor0.076 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.15 23°C/100 Hz; IEC 60250
Comparative Tracking Index600 V Test Solution A; IEC 60112

Thermal Properties
CTE, linear 20°C160 µm/m-°C 23-55°C, Longitudinal; ISO 11359
CTE, linear 20°C160 µm/m-°C 23-55°C, Transverse; ISO 11359
Deflection Temperature at 0.46 MPa (66 psi)100 °C ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi)45 °C ISO 75-1
Vicat Softening Point130 °C 50N; ISO 306
Vicat Softening Point170 °C 10N; ISO 306
Flammability, UL94HB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.