Degussa AG Vestamid® L1670 Nylon 12 for Fiber Optic Jacketing


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Material Notes:
Description: L1670 is a semi-crystalline PA 12 grade of low melt viscosity; exhibiting very good flow characteristics. This grade offers consistent protection of the glass fiber against microbending and strain. Recommended for tight buffering.

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ ISO 1183
Water Absorption at Saturation1.4 %1.4 % ISO 62
Melt Flow60.6 g/10 min60.6 g/10 min 250°C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Shore D7171 ISO 868
Tensile Strength, Yield45 MPa6530 psi ISO 527-2/1A
Elongation at BreakMin 50 %Min 50 % ISO 527-2/1A
Elongation at Yield6 %6 % ISO 527-2/1A
Tensile Modulus1.4 GPa203 ksi ISO 527-1/2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.5 J/cm²2.38 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, Notched0.4 J/cm²1.9 ft-lb/in² 23°C; ISO 179/1eA

Thermal Properties
CTE, linear 20°C150 µm/m-°C83.3 µin/in-°F 23-80°C; ISO 11359
Melting Point175 - 178 °C347 - 352 °F DSC

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.