Degussa AG Vestamid® L1670 Nylon 12 for Fiber Optic Jacketing
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Material Notes: Description: L1670 is a semi-crystalline PA 12 grade of low melt viscosity; exhibiting very good flow characteristics. This grade offers consistent protection of the glass fiber against microbending and strain. Recommended for tight buffering. Information provided by degussa.
Physical Properties | Original Value | Comments |
|
Density | 1.01 g/cc | ISO 1183 |
Water Absorption at Saturation | 1.4 % | ISO 62 |
Melt Flow | 60.6 g/10 min | 250°C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Shore D | 71 | ISO 868 |
Tensile Strength, Yield | 45 MPa | ISO 527-2/1A |
Elongation at Break | Min 50 % | ISO 527-2/1A |
Elongation at Yield | 6 % | ISO 527-2/1A |
Tensile Modulus | 1.4 GPa | ISO 527-1/2 |
Charpy Impact Unnotched | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.5 J/cm² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 0.4 J/cm² | 23°C; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 150 µm/m-°C | 23-80°C; ISO 11359 |
Melting Point | 175 - 178 °C | DSC |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|