Degussa AG Vestamid® L2124 Plasticized Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12-P, EHL,22-004

Material Notes:
Description: High-viscosity, plasticized, heat- and light-stabilized, with processing aid

Applications: Fuel, vacuum and hydraulic lines, sheathing of steel cables

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.03 g/cc ISO 1183
Moisture Absorption at Equilibrium0.5 % 23°C/50% R.H. (1mm); ISO 62
Linear Mold Shrinkage0.013 cm/cm 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.016 cm/cm 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength, Yield26 MPa ISO 527-1/2
Elongation at BreakMin 50 % ISO 527-1/2
Elongation at Yield31 % ISO 527-1/2
Tensile Modulus0.4 GPa ISO 527-1/2
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.6 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched15 J/cm² 23°C, Partial Break; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+012 ohm-cm IEC 60093
Dielectric Constant3.8 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency12 23°C/100 Hz; IEC 60250
Dielectric Strength31 kV/mm K20/P50; IEC 60243-1
Dissipation Factor0.15 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.16 23°C/100 Hz; IEC 60250
Comparative Tracking IndexMin 600 V Test Solution A, 50 drops; IEC 60112
Comparative Tracking Index600 V Test Solution A, 100 drops; IEC 60112

Thermal Properties
CTE, linear 20°C180 µm/m-°C 23-55°C (45x15x10 mm); ISO 11359
Melting Point171 °C Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)90 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)45 °C ISO 75
Vicat Softening Point125 °C 50N; ISO 306
Vicat Softening Point165 °C 10N; ISO 306
Flammability, UL94HB 3.2 mm
Flammability, UL94HB 1.6 mm

Descriptive Properties
ColorBlack 
Electrolytic CorrosionA1 Step IEC 60426

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.