Degussa AG Vestamid® L2140 Black Nylon 12 for Fiber Optic Jacketing
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Material Notes: Description: L2140 black is a PA 12 grade of high melt viscosity and excellent weatherability. Cables with a covering layer of L2140 are protected against damage from ants and termites. Information provided by degussa.
Physical Properties | Metric | English | Comments |
|
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
Water Absorption at Saturation | 1.5 % | 1.5 % | ISO 62 |
Melt Flow | 36.72 g/10 min | 36.72 g/10 min | 250°C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Shore D | 73 | 73 | ISO 868 |
Tensile Strength, Yield | 45 MPa | 6530 psi | ISO 527-2/1A |
Elongation at Break | Min 50 % | Min 50 % | ISO 527-2/1A |
Elongation at Yield | 5 % | 5 % | ISO 527-2/1A |
Tensile Modulus | 1.4 GPa | 203 ksi | ISO 527-1/2 |
Charpy Impact Unnotched | NB | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.9 J/cm² | 4.28 ft-lb/in² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | NB | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 1.6 J/cm² | 7.61 ft-lb/in² | 23°C; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 140 µm/m-°C | 77.8 µin/in-°F | 23-80°C; ISO 11359 |
Melting Point | 175 - 178 °C | 347 - 352 °F | DSC |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|