Degussa AG Vestamid® L2140 Black Nylon 12 for Fiber Optic Jacketing


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Material Notes:
Description: L2140 black is a PA 12 grade of high melt viscosity and excellent weatherability. Cables with a covering layer of L2140 are protected against damage from ants and termites.

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.02 g/cc ISO 1183
Water Absorption at Saturation1.5 % ISO 62
Melt Flow36.72 g/10 min 250°C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Shore D73 ISO 868
Tensile Strength, Yield45 MPa ISO 527-2/1A
Elongation at BreakMin 50 % ISO 527-2/1A
Elongation at Yield5 % ISO 527-2/1A
Tensile Modulus1.4 GPa ISO 527-1/2
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.9 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched1.6 J/cm² 23°C; ISO 179/1eA

Thermal Properties
CTE, linear 20°C140 µm/m-°C 23-80°C; ISO 11359
Melting Point175 - 178 °C DSC

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.